BULK
DENSITY(g/cm³)/ ( RELATIVE DENSITY %)
|
3.10~3.15/
(97~98) |
COMPRESSIVE STRENGTH (Kg/mm²)
At Room Temp. |
170~190
|
YOUNG’S MODULES (x10Kg/mm²) At Room Temp. |
2.9~3.1
|
K1C-VALVE (MN/m3/2)
[FRACTURE TOUGHNESS] |
5.3 |
VICKERS HARDNESS (Kg/mm²)
AT ROOM TEMP. |
1400~1550 |
FRICTION FACTOR (CERAMICS
TO CERAMICS) |
0.6 |
THERMAL EXPANSION
COEFFICIENT (x10-7/°C) |
33~35 |
THERMAL CONDUCTIVITY (Kcal/mh°C)
AT 100°C |
16~17 |
THERMAL SPALLING RESISTANCE
(°C) |
750~800 |
WEIGHT INCREASE BY OXIDATION IN AIR (mg/cm²) AT
1,200°C x 24 hours
AT 1,400°C x 24 hours |
0.2~0.5
_ |
ELECTRICAL RESISTIVITY (W·cm)
At Room Temp.
At 1,000°C |
>1016
1013~1014 |